Tantalum Capillary Tube Micro Tube

Tantalum Capillary Tube Micro Tube

Tantalum capillary tube is a kind of tube made of tantalum material, which is widely used in various industries.
Отправить запрос
Теперь говорите
Описание

 

Products Description Tel:400-010-0000

Features:

Tantalum capillary tube has an excellent heat resistance and corrosion resistance. It can work stably and reliably in many harsh environments such as high temperatures and high pressure. At the same time, it also has good electrical insulation, good weldability, and excellent mechanical properties.

The tantalum tube has excellent physical, chemical, and mechanical properties, stable performance, and strong anti-corrosion abilities, especially for withstanding high temperatures and pressure. it also offers high wear resistance, low thermal expansion coefficient, and inertness to most chemical agents.

tantalum capillary tube micro tube R05200
Specification Tel:0917-3664600
Grade Ta1  R05200 Ta2 R05400
Size 6.35X0.55 6.6X0.4
Standards 138*188 37*37*148
Queen 153*203 37*37*163
King 183*203 37*37*193
Factory Tour Tel:0917-3664600
tantalum capillary tube micro tube in stock
tantalum capillary tube micro tube manufacture
tantalum capillary tube micro tube R05200
Manufacture process of tantalum capillary tube  Tel:0917-3664600

Tantalum capillary tube is manufactured by a special process. Firstly, tantalum material is rolled into a sheet and then cut into required lengths. After that, the sheet is cold drawn into a tube and the wall of the tube is precisely adjusted to the required thickness. Finally, the tube is further processed and processed to its final specifications.

Applications of tantalum capillary tube micro tube Tel:0917-3664600

Tantalum capillary tube is manufactured by a special process. Firstly, tantalum material is rolled into a sheet and then cut into required lengths. After that, the sheet is cold drawn into a tube and the wall of the tube is precisely adjusted to the required thickness. Finally, the tube is further processed and processed to its final specifications.

Packing And Shipping Tel:0917-3664600

details4-5.jpg

details4-6.jpg

горячая этикетка : tantalum capillary tube micro tube, China, suppliers, manufacturers, factory, customized, wholesale, bulk, low price, for sale, in stock, buy discount, made in China

Отправить запрос
Категории продуктов

(0/10)

clearall